Preparation of WC cemented carbide without metallic binder toughened by MgO-B2O3 via spark plasma sintering at 1400℃

In order to reduce the sintering temperature and obtain higher fracture toughness of WC cemented carbides without metallic binder, WC cemented carbide was toughened by MgO and B2O3. Dense WC-MgO-B2O3 bulk materials were prepared at the relative low temperature of 1400℃ via spark plasma sintering(SPS...

Full description

Bibliographic Details
Main Authors: LAI Jiaming, LI Jingmao, ZHU Dezhi, LIANG Liang, QU Shengguan, LI Xiaoqiang
Format: Article
Language:zho
Published: Journal of Materials Engineering 2022-11-01
Series:Cailiao gongcheng
Subjects:
Online Access:http://jme.biam.ac.cn/CN/10.11868/j.issn.1001-4381.2021.000441