Strength–ductility balance of powder metallurgy Ti–2Fe–2W alloy extruded at high-temperature
This study aims to improve the mechanical properties of a Ti–2Fe base alloy by adding W solute and performing hot extrusion at a high temperature (1000 °C). W was added at 0, 1, 2, and 3 wt% using the powder metallurgy route and homogenization heat treatment. The as-extruded materials predominantly...