Manufacturing of Refractory Bricks from Iraqi Flint
It was done in this study the preparation of bricks refractory from Iraqi Flint and adding Iraqi white kaolin as a binding material in ratio (25, 30, 35, 40, 45)%. The samples were formed by dry pressing, dried at room temperature for 24hr then at (110)̊C for 6hr then fired at (1200)˚C with soking t...