Oxidation behavior of Al2O3 added reaction-sintered SiC ceramics in wet oxygen environment at 1300°C

The oxidation behavior of reaction-bonded SiC ceramics with Al2O3 was investigated at 1300°C for exposure duration up to 100 h under water vapor environment. Results show that Al2O3 is enriched on the oxidation surface, reducing the volatilization of the oxide layer and preventing the reduction of m...

Full description

Bibliographic Details
Main Authors: Qingliang Shan, Jianbao Hu, Jinshan Yang, Yanmei Kan, Haijun Zhou, Guangxiang Zhu, Yudong Xue, Shaoming Dong
Format: Article
Language:English
Published: Taylor & Francis Group 2018-07-01
Series:Journal of Asian Ceramic Societies
Subjects:
Online Access:http://dx.doi.org/10.1080/21870764.2018.1504731