Oxidation behavior of Al2O3 added reaction-sintered SiC ceramics in wet oxygen environment at 1300°C
The oxidation behavior of reaction-bonded SiC ceramics with Al2O3 was investigated at 1300°C for exposure duration up to 100 h under water vapor environment. Results show that Al2O3 is enriched on the oxidation surface, reducing the volatilization of the oxide layer and preventing the reduction of m...
Main Authors: | Qingliang Shan, Jianbao Hu, Jinshan Yang, Yanmei Kan, Haijun Zhou, Guangxiang Zhu, Yudong Xue, Shaoming Dong |
---|---|
Format: | Article |
Language: | English |
Published: |
Taylor & Francis Group
2018-07-01
|
Series: | Journal of Asian Ceramic Societies |
Subjects: | |
Online Access: | http://dx.doi.org/10.1080/21870764.2018.1504731 |
Similar Items
-
Self lubrication of pressureless sintered SiC ceramics
by: Wei Zhang, et al.
Published: (2020-11-01) -
Preparation of biomorphic SiC ceramics
by: Egelja A., et al.
Published: (2008-01-01) -
Combination of PIP and LSI processes for SiC/SiC ceramic matrix composites
by: Fabia Süß, et al.
Published: (2021-03-01) -
Structure and Properties of Spark Plasma Sintered SiC Ceramics with Oxide Additives
by: Dauren Zhambakin, et al.
Published: (2023-07-01) -
SiC/SiC ceramic matrix composites with BN interphase produced by gas phase routes: An overview
by: Pierre Fenetaud, et al.
Published: (2023-09-01)