Achievement of excellent strength and plasticity in the nugget zone of friction stir welded bainitic steel and its deformation behavior

Compared to nonferrous alloy, the microstructure in the nugget zone (NZ) of steel is easy to coarsen during friction stir welding (FSW) because of higher melting point of steel, leading to lower strength and plasticity of the joint. Here, high-strength bainitic steel was subjected to FSW in water + ...