Hot Corrosion of Co-based Alloys with 25%NaCl+75%Na2SO4 Coating at 1173 K
Hot corrosion behavior of pure Co, Co-10Cr and Co-10Cr-5Al alloys in the presence of a salt coat of Na2SO4+NaCl in air at 1173 K was studied. The results indicated that among the three samples, the mass gain of Co-10Cr-5Al alloy is the smallest, while that of Co-10Cr is biggest. The corrosion produc...