Durability of blast-furnace slag concrete mixed with expansive and swelling admixtures

South Korean concrete crack management standards deem cracks larger than 0.3 mm to be defects. However, concrete crack reduction technology is lacking and urgently needed to meet these standards. In this study, the durability characteristics of blast-furnace slag concrete with an expansion material...