Effect of ball milling time on corrosion and wear resistance of Ti-13Nb-5Sn dental alloys

Ti-13Nb-5Sn dental alloy was prepared by powder metallurgy method. The effects of ball milling time (3, 12, 24 h and 48 h) on powder performances, material microstructure, electrochemical corrosion and tribological behavior were investigated. The results show that with the increase of ball milling t...

Full description

Bibliographic Details
Main Authors: XIE Fangxia, LU Dongxing, HUANG Jiabing, ZHANG Wencheng, SUN Qichao, HE Xueming
Format: Article
Language:zho
Published: Journal of Materials Engineering 2024-03-01
Series:Cailiao gongcheng
Subjects:
Online Access:http://jme.biam.ac.cn/CN/10.11868/j.issn.1001-4381.2022.000449