Effect of Rolling Temperature on the Microstructure and Mechanical Properties of Mg-2Zn-0.4Y Alloy Subjected to Large Strain Rolling

Large strain rolling (LSR) has been conducted on the Mg-2Zn-0.4Y alloy. After the 1st rolling process at 250, 300, 350, and 400 °C, the alloy demonstrates a fully recrystallized microstructure. The grain size increases from 6, 8, 12, to 17 μm with an increasing rolling temperature....