Effect of Carbides on Thermos-Plastic and Crack Initiation and Expansion of High-Carbon Chromium-Bearing Steel Castings

The bearing steel’s high-temperature brittle zone (1250 °C–1100 °C), second brittle zone (1100 °C–950 °C), and low-temperature brittle zone (800 °C–600 °C) were determined by the reduction in area and true fracture toughness. The crack sensitivity was strongest at temperatures of 1200 °C, 1000 °C, a...