CORROSION RESISTANCE OF SELF-COMPACTING CONCRETE CONTAINING CALCIUM STEARATE
This study aims to determine the corrosion resistance of self-compacting concrete (SCC) combined with calcium stearate (CS), Ca(C18H35O2)2. The concrete qualities tested are 20, 30, and 40 MPa. The CS dose used ranges from 0 to 2.85% of the cement weight. Two types of testing were performed in this...
Główni autorzy: | AGUS MARYOTO, BUNTARA STHENLY GAN, NOR INTANG SETYO HERMANTO, RACHMAD SETIJADI |
---|---|
Format: | Artykuł |
Język: | English |
Wydane: |
Taylor's University
2018-10-01
|
Seria: | Journal of Engineering Science and Technology |
Hasła przedmiotowe: | |
Dostęp online: | http://jestec.taylors.edu.my/Vol%2013%20issue%2010%20October%202018/13_10_19.pdf |
Podobne zapisy
-
Drying Shrinkage of Concrete Containing Calcium Stearate, (Ca(C<sub>18</sub>H<sub>35</sub>O<sub>2</sub>)<sub>2</sub>), with Ordinary Portland Cement (OPC) as a Binder: Experimental and Modelling Studies
od: Agus Maryoto, i wsp.
Wydane: (2020-10-01) -
Evaluation of corrosion inhibition effect of glycerol stearate on aluminium metal by electrochemical techniques
od: Thabo Pesha, i wsp.
Wydane: (2023-07-01) -
Kesan kalsium stearat sebagai pelincir terhadap kebolehprosesan plastik kitar semula /
od: 340967 Nur Fadzeelah Abu Kassim
Wydane: (2000) -
Thermal degradation kinetics of calcium stearate/PVC composite
od: Wang Guangbao, i wsp.
Wydane: (2020-12-01) -
Thermal evaluation of the calcium stearate influence on polystyrene by in-line colorimetry
od: Felipe Bernardo, i wsp.
Wydane: (2024-05-01)