Influence of directional solidification variables on primary dendrite arm spacing of Ni-based superalloy DZ125
The primary dendrite morphology and spacing of DZ125 superalloy have been observed during directional solidifi cation under high thermal gradient about 500 K/cm. The results reveal that the primary dendrite arm spacing decreases from 94 μm to 35.8 μm with the increase of directional solidifi cation...