On the early stages of localised atmospheric corrosion of magnesium–aluminium alloys
The surface film on pure magnesium and two aluminium-containing magnesium alloys was characterised after 96 h at 95% RH and 22 °C. The concentration of CO₂ was carefully controlled to be either 0 or 400 ppm. The exposed samples were investigated using X-ray photoelectron spectroscopy, Fourier transf...