DOPING EFFECTS ON INDENTATION PLASTICITY AND FRACTURE IN GERMANIUM

Vickers micro-indentation tests have been performed in the temperature range 20 to 420° C on the {0 0 1} surfaces of germanium crystals of three different dopings: "intrinsic", heavily doped p-type and heavily doped n-type. Indentation sizes, dislocation rosette sizes and median/radial cra...

Full description

Bibliographic Details
Main Authors: Roberts, S, Pirouz, P, Hirsch, P
Format: Journal article
Language:English
Published: Kluwer Academic Publishers 1985