Observation of internal oxidation in a 20% cold-worked Fe-17Cr-12Ni stainless steel through high-resolution characterization

It is often assumed that internal oxidation cannot occur at temperatures below 400ºC. However, in the present work, internal oxidation was observed in a 20% cold-worked Fe-17Cr-12Ni stainless steel (SS) after exposure to simulated primary water of a pressurized water reactor at 340ºC and not in a si...

Full description

Bibliographic Details
Main Authors: Shen, Z, Tweddle, D, Lapington, M, Jenkins, BM, Du, D, Zhang, L, Moody, M, Lozano-Perez, S
Format: Journal article