Strain rate dependence of mode II delamination resistance in through thickness reinforced laminated composites
<p>A thorough experimental procedure is presented in which the mode II delamination resistance of a laminated fibre reinforced plastic (FRP) composite with and without Z-pins is characterised when subjected to increasing strain rates. Standard three-point End Notched Flexure (3ENF) specimens w...
Main Authors: | Yasaee, M, Mohamed, G, Pellegrino, A, Petrinic, N, Hallett, SR |
---|---|
Format: | Journal article |
Published: |
Elsevier
2017
|
Similar Items
-
Dynamic mode II delamination in through thickness reinforced composites
by: Yasaee, M, et al.
Published: (2016) -
Dynamic bridging mechanisms of through-thickness reinforced composite laminates in mixed mode delamination
by: Cui, H, et al.
Published: (2017) -
Bridging mechanisms of through-thickness reinforcement in dynamic mode I&II; delamination
by: Cui, H, et al.
Published: (2017) -
Mode II delamination resistance of composites reinforced with inclined Z-pins
by: Beene M'membe, et al.
Published: (2016-03-01) -
Effect of delamination interface angle on Mode Ⅱ delamination behavior of CFRP laminates
by: ZHAO Wei, et al.
Published: (2019-09-01)