The strength of Al2O3/SiC nanocomposites after grinding and annealing
Alumina matrix nanocomposites containing about 5 vol.% SiC of < 100 nm mean particle size show a substantial increase in strength after machining and annealing. The final strength is controlled by the annealing process and achieves the same level after a coarse machining using 150-grit diamon...
मुख्य लेखकों: | Wu, H, Lawrence, C, Roberts, S, Derby, B |
---|---|
स्वरूप: | Conference item |
प्रकाशित: |
1998
|
समान संसाधन
-
Erosion resistance of hot pressed Al2O3/SiC nanocomposites
द्वारा: Lawrence, C, और अन्य
प्रकाशित: (1998) -
Erosive wear of alumina/SiC nanocomposite ceramics
द्वारा: Lawrence, C, और अन्य
प्रकाशित: (1999) -
Crack healing in an alumina/silicon carbide nanocomposite after grinding and annealing
द्वारा: Wu, H, और अन्य
प्रकाशित: (2000) -
Residual stress distributions around indentations and scratches in polycrystalline Al2O3 and Al2O3/SiC nanocomposites measured using fluorescence probes
द्वारा: Wu, H, और अन्य
प्रकाशित: (2008) -
Wet erosion behaviour of low SiC alumina-SiC nanocomposites
द्वारा: Kara, H, और अन्य
प्रकाशित: (2002)