Grain size dependence of hardness and fracture toughness in pure near fully-dense boron carbide ceramics
Room temperature fracture toughness and hardness of spark plasma sintered pure B4C ceramics with grain sizes ranging from 120 nm to 17 μm have been studied. Vickers indentation and single edge V-notched beam (SEVNB) techniques have been used to measure hardness and fracture toughness, respectively....
Главные авторы: | Moshtaghioun, BM, Gomez-Garcia, D, Dominguez-Rodriguez, A, Todd, RI |
---|---|
Формат: | Journal article |
Язык: | English |
Опубликовано: |
European Ceramic Society
2016
|
Схожие документы
-
Abrasive wear rate of boron carbide ceramics: Influence of microstructural and mechanical aspects on their tribological response
по: Moshtaghioun, B, и др.
Опубликовано: (2016) -
Tough and dense boron carbide obtained by high-pressure (300 MPa) and low-temperature (1600°C) spark plasma sintering
по: Badica, Petre, и др.
Опубликовано: (2014) -
Importance of hardness and toughness in ceramic armour
по: Goh, Wei Liang
Опубликовано: (2019) -
Fracture Toughness and Hardness studying for Polymer-Ceramic Composite
по: Baghdad Science Journal
Опубликовано: (2014-06-01) -
Effect of glazing and thermocycling on the fracture toughness and hardness of a New fully crystallized aluminosilicate CAD/CAM ceramic material
по: Ahmed Mahmoud Fouda, и др.
Опубликовано: (2024-05-01)