Properties of Si3N4-TiN composites fabricated by spark plasma sintering by using a mixture of Si3N4 and Ti powders
Si3N4–TiNcomposites were successfully fabricated via planetary ball milling of 70 mass% Si3N4 and 30 mass% Tipowders, followed by sparkplasmasintering (SPS) at 1250–1350 °C. The sintering mechanism for SPS was a hybrid of dissolution–reprecipitation and viscous flow. The electrical resistivity decre...